AWS ER5183 Aluminom Welding Waya Aluminom MIG welding Rods Tig Waya

Nkọwa dị mkpirikpi:

ER5183 dabara maka MIG ịgbado ọkụ aluminum magnesium alloy na elu tensile ike chọrọ ma ọ bụrụ na isi metal bụ 5083 ma ọ bụ 5654 ike tensile ga-adị elu nke ukwuu.A na-eji ya eme ihe maka ịgbado ọkụ aluminom magnesium alloy nke ụgbọ mmiri, ọdụ ụgbọ mmiri, ụgbọ ala & ụgbọ ala, ụgbọ ala, arịa, ụgbọ mmiri cryogenic na ndị ọzọ.


Nkọwa ngwaahịa

Mkpado ngwaahịa

ER5183 dabara maka MIG ịgbado ọkụ aluminum magnesium alloy na elu tensile ike chọrọ ma ọ bụrụ na isi metal bụ 5083 ma ọ bụ 5654 ike tensile ga-adị elu nke ukwuu.A na-eji ya eme ihe maka ịgbado ọkụ aluminom magnesium alloy nke ụgbọ mmiri, ọdụ ụgbọ mmiri, ụgbọ ala & ụgbọ ala, ụgbọ ala, arịa, ụgbọ mmiri cryogenic na ndị ọzọ.Igwe weld ya nwere ezigbo nguzogide brine corrosion.

Ọnọdụ ịgbado ọkụ: F, HF, V

Ụdị nke ugbu a: DCEP

IHE:

Idobe ngwugwu nke waya ahụ n'ọnọdụ dị mma tupu ịgbado ọkụ.

A ga-ehichapụrịrị ma ihe ndị a ga-eji weld weld na waya gbachie adịghị ọcha nke mmetọ mmanụ, mkpuchi oxide, mmiri mmiri na ihe ndị ọzọ.

Iji nweta ọdịdị dị mma nke weld ọ dị mkpa ka preheat isi metal ka 100 ℃-200 ℃ tupu ịgbado ọkụ ma ọ bụrụ na ya ọkpụrụkpụ bụ 10mm ma ọ bụ karịa.

Ọ ka mma itinye subplate n'okpuru weld mpaghara iji kwado metal gbazere ka o wee hụ na ntinye nke weldment zuru oke.

Dị ka ịgbado ọkụ ọnọdụ na ọkpụrụkpụ nke isi metal dị iche iche ọta gas ga-ahọrọ, dị ka 100% Ar, 75% Ar + 25% He, 50% Ar + 50% He, wdg.

Ọnọdụ ịgbado ọkụ ahụ a kpọtụrụ aha n'elu maka ntụaka naanị na ọ ka mma ịme ntozu usoro ịgbado ọkụ dị ka ọrụ siri dị tupu etinye ya n'ụdị ịgbado ọkụ.

ER5183 Ngwakọta kemịkal nke ọla edobere (%):

SI FE CU MN MG CR ZN TI AI BE
Ọkọlọtọ ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 Nhazi ≤0.0003
Ụdị 0.08 0.12 0,006 0.65 4.75 0.130 0,005 0.080 Nhazi 0,0001

AKWỤKWỌ NGWA NKE ỌLA KWESỊRỊ (AW):

Ike TENSILE RM (MPA) IKE REL (MPA) ELONGATION A4 (%)
Ụdị 280 150 18

Nha na akwadoro ugbu a maka MIG (DC+):

MMỤTA WIRE NDỊ MMADỤ (MM) 1.2 1.6 2.0
Welding ugbu a (A) 180-300 200-400 240-450
Voltaji ịgbado ọkụ (V) 18-28 20-20 22-34

Nha & akwadoro ugbu a maka TIG (DCn):

MMỤTA WIRE NDỊ MMADỤ (MM) 1.6-2.5 2.5-4.0 4.0-5.0
Welding ugbu a (A) 150-250 200-320 220-400